Douglas Fir is a difficult wood to stain evenly. A 50|50 mix of your Exterior 450 stain color and Exterior 450 Clear would be a better choice for an exterior conditioner. Blotching may still occur even with this procedure.

After applying the conditioner mix, let it dry 2-3 hours. Allow more time in humid weather. Then a apply the stain color of your choice. Multiple coats will deepen the color.

Pre-Stain Wood Conditioner with an oil-based stain is designed for use before staining new, soft, and porous wood surfaces, such as aspen, cherry, birch, poplar, or pine.

Water-Based Pre-Stain Conditioner is a formula similar to our water-based stains without the colorant. Before applying a water-based wood stain, use General Finishes Pre-Stain Conditioner Natural to control blotching on hard-to-stain woods, such as maple, pine, and cherry.

Maple is one of the most difficult woods to achieve a dark, uniform stain color on because it is a dense, closed grain wood and often absorbs stain very unevenly. General Finishes Gel Stains or Water Based Stains usually will perform very well because they are more topical than traditional liquid oil stains, and contain more colorants. 

General Finishes offers a complete line of oil based, water based and wax products. Application techniques differ between oil based products and water based products.

There are several reasons to choose Dye Stain. Here are a few.

Hand Application of General Finishes Water Based Wood Stains

  • Always stir the contents well.

Decorative Finishes- Distressing, Antique Finishes, Faux Marble and More

All bright white paint will yellow slightly with time, even without topcoat. You have probably tried to touch up white woodwork in your home after several years and noticed that the new paint is brighter.

But white and light paints can react if clear coated with a waterbased finish; water-based topcoats are reactive and may draw out substances in the wood such as tannins, dyes or unknown substances in existing finishes causing the topcoat to yellow. This is an industry-wide issue and can happen right away, years later or never.