The most critical part of finishing a piece of furniture happens before you open a can of stain or paint - it starts with the sanding. Sanding is critical to creating a smooth surface. Use the following sanding sequences for new wood:

PAINT

For wood that is going to be painted, use 120-grit, followed by 150-grit.

It is normal to see a bit of stain on the brush when applying the first coat of topcoat. Topcoats often pull a bit of color on the first pass, but good preparation will minimize this.

To prepare open grains woods such as raw Oak for a water-based stain, we recommend sanding with 180-grit followed by no more than 220-grit sandpaper.