Gel Stain is engineered for wood, but it has successfully adhered to more surfaces than we could have imagined. However, since tile cannot be abraded properly though sanding,  lasting adhesion may be difficult if not impossible. 

Milk Paint will have a better chance of adhering than Gel Stain. Dark Chocolate Milk Paint was created to match the color of Java Gel stain, for example. Both products are more likely to adhere if they are applied over a tile-appropriate primer. 

You can apply Gel Stain to MDF, stained surfaces

GF advises extra care and prep when applying any finish over laminate surfaces because they are specifically designed not to mar and therefore they are not very "sand-able", making adherence difficult.

In addition to this non-permeable surface factor, General Finishes Gel Stain is an oil-based product, and it is more difficult to obtain proper drying characteristics over a dense manufactured surface such as laminate. Gel stains, as all wood stains, were formulated to go over raw wood which has an "open" surface and can absorb some of the stain.

Gel Stain can be mixed with up to 50% Liquid Oil Stain but be aware that this will thin the viscosity.

We recommend starting with 10% Liquid Oil Stain and testing to your satisfaction. Add more Liquid Stain as needed up to 50%. The mix will be thin and more translucent with less color saturation and intensity, but will not lose any of its properties for adhesion and curing.

General Finishes offers a complete line of oil based, water based and wax products. Application techniques differ between oil based products and water based products.

We love this unique fireplace makeover, for less than $20, by Cassie from Primitive & Proper, using General Finishes Lamp Black

As the Gel Stain is used, the volume of stain in the can is displaced with air, causing the stain to start curing. Gel Stains harden up more quickly than liquid oil stains for all the reasons folks love them - the extra colorants and solids within the stain that provide such great coverage also harden up more quickly than other stains.

During storage, the oxygen or moisture that's sealed in the container continues to cure and thicken your stored product, ruining the leftovers. Here are some tips to ensure your Gel Stain remains in great working condition.

ANSWER

Haze (the technical term is blush) is caused by too many coats applied too quickly. A recoat time of 12 hours is not enough dry time when applying over an EXISTING finish. To remove the blush or haze, you can either wipe the area with a strong solvent, like xylene or lacquer thinner, or you can try sanding out the haze and then reapply the topcoat.

Gel Stain from General Finishes is home of the popular Java Gel Stain featured across the nation's social media for upcycling furniture and cabinets.