As the Gel Stain is used, the volume of stain in the can is displaced with air, causing the stain to start curing. Gel Stains harden up more quickly than liquid oil stains for all the reasons folks love them - the extra colorants and solids within the stain that provide such great coverage also harden up more quickly than other stains.

During storage, the oxygen or moisture that's sealed in the container continues to cure and thicken your stored product, ruining the leftovers. Here are some tips to ensure your Gel Stain remains in great working condition.

In this latest video, Chris Adams of General Finishes shows you 7 great tips for getting the most mileage out of a leftover can of finish after use.  

GF advises extra care and prep when applying any finish over laminate surfaces because they are specifically designed not to mar and therefore they are not very "sand-able", making adherence difficult.

In addition to this non-permeable surface factor, General Finishes Gel Stain is an oil-based product, and it is more difficult to obtain proper drying characteristics over a dense manufactured surface such as laminate. Gel stains, as all wood stains, were formulated to go over raw wood which has an "open" surface and can absorb some of the stain.

It's always possible to darken a stained surface, but you cannot lighten a stained surface after the finish has dried.

When the surface is still wet, you can try to lighten the color by scrubbing with mineral spirits. If the finish has hardened, you will need to sand down your current stain and start over or use one of our paints.

You can mix GF Gel Stain colors to create a custom color.

You can also thin Gel Stain with 10-15% mineral spirits.

Always test our color on a hidden area of your project before beginning.

Haze (the technical term is blush) is caused by too many coats applied too quickly. A recoat time of 12 hours is not enough dry time when applying over an EXISTING finish. To remove the blush or haze, you can either wipe the area with a strong solvent, like xylene or lacquer thinner, or you can try sanding out the haze and then reapply the topcoat.

Gel Stain can be mixed with up to 50% Liquid Oil Stain but be aware that this will thin the viscosity.

We recommend starting with 10% Liquid Oil Stain and testing to your satisfaction. Add more Liquid Stain as needed up to 50%. The mix will be thin and more translucent with less color saturation and intensity, but will not lose any of its properties for adhesion and curing.

Enduro-Var sprays beautifully if the gun is absolutely clean and does not have any other finish residue. Proper cleaning with acetone followed with hot water should purge the fluid passage. Enduro-Var itself will not cause gun failure.

Another possibility is the power of the gun. Some of the lower quality guns can overheat causing the product to cure in the gun - they need a rest once in a while if you are using them all day.

Also note that Enduro-Var ADHERES WELL only over WATER STAINS, DYE STAINS, and RAW WOOD.

General Finishes is often asked about product cans. Why do they rust? Why aren't they made of plastic? Here is the backstory:

During the supply-line shortages caused by Covid, we are thrilled to have any cans for our paints, stains, and topcoats.

There are several reasons:

1. The cabinets were not prep cleaned and sanded properly. Sanding and cleaning are an essential part of any refinishing process.

In most cases, you can use a 220 sanding pad to scuff the surface and clean with a 50|50 mix of water and denatured alcohol.

Ideal Conditions are 70 degrees F and 50% humidity. Refinishing furniture in a space that is below or above the 65-75 degrees F range can lead to problems, and a space below 55 degrees F is definitely too cold.

WATER-BASED TOPCOATS

One issue caused by cold temperatures with water-based topcoats is the development of dimples in the finish called Orange Peel.